Skip to main navigation Skip to search Skip to main content

Warp and weft direction damage development in the late-stage fatigue life of a 3D non-crimp orthogonal weave composite

  • M. C. Poole
  • , S. L. Ogin
  • , P. A. Smith
  • , G. M. Wells
  • , P. Potluri
  • , P. J. Withers

Research output: Chapter in Book/Report/Conference proceeding › Conference Paper › Other

Abstract

The development of damage throughout the fatigue lifetime of specimens loaded along the warp and weft directions of a three-directional non-crimp orthogonal woven (3DNCOW) composite has been studied in detail. The fundamental damage mechanisms are, not surprisingly, common to each direction (i.e. transverse cracks, interfacial debonding (Z-binder debonding, micro-delaminations) and longitudinal splits). However, the difference of fibre architecture in relation to the loading direction leads to minor differences in the details of the damage for the two loading directions. In particular, there is an increased crack density, a delay in the formation of delaminations, and a slight difference in the initiation location of Z-binder debonds, and longitudinal splits, in weft direction loaded specimens when compared to warp direction loaded specimens.

Original languageEnglish
Title of host publicationECCM 2016 - Proceeding of the 17th European Conference on Composite Materials
PublisherEuropean Conference on Composite Materials, ECCM
ISBN (Electronic)9783000533877
Publication statusPublished - 2016
Externally publishedYes
EventEuropean Conference on Composite Materials 2016 - Munich, Germany
Duration: 26 Jun 2016 → 30 Jun 2016
Conference number: 17th
https://www.carbon-connected.de/Group/ECCM17.-.17th.European.Conference.on.Composite.Materials/GroupOverview

Conference

ConferenceEuropean Conference on Composite Materials 2016
Abbreviated titleECCM 2016
Country/TerritoryGermany
CityMunich
Period26/06/16 → 30/06/16
Internet address

Keywords

  • 3D woven composites
  • Damage development
  • Fatigue

Cite this