Stress Corrosion Cracking Susceptibility of Mild Steel and Stainless Steels in Caustic Environments

Research output: Chapter in Book/Report/Conference proceedingConference PaperResearchpeer-review

Original languageEnglish
Title of host publicationCorrosion & Prevention 02, Proceedings
EditorsM Ali
Place of PublicationBrentford Square Vic Australia
PublisherAustralasian Corrosion Association
Pages084/1 - 084/6
Number of pages6
Publication statusPublished - 2002
EventAustralasian Corrosion Association (ACA) Conference 2002: Corrosion and Prevention - Adelaide , Australia
Duration: 10 Nov 200213 Nov 2002
Conference number: 42nd

Conference

ConferenceAustralasian Corrosion Association (ACA) Conference 2002
Abbreviated titleCP 2002
CountryAustralia
CityAdelaide
Period10/11/0213/11/02