Stress Corrosion Cracking of Steels in Aggressive Caustic Solutions

Research output: Chapter in Book/Report/Conference proceedingConference PaperResearchpeer-review

Original languageEnglish
Title of host publicationEngineering Materials 2001
EditorsE V Pereloma, K Raviprasad
Place of PublicationMelbourne Vic Australia
PublisherThe Institute of Materials Engineering Australasia
Pages251 - 256
Number of pages6
ISBN (Print)187-658-511-8
Publication statusPublished - 2001
EventEngineering Materials Institute of Materials Engineering Australasia (IMEA) - Melbourne Australia, Melbourne Vic Australia
Duration: 1 Jan 2001 → …

Conference

ConferenceEngineering Materials Institute of Materials Engineering Australasia (IMEA)
CityMelbourne Vic Australia
Period1/01/01 → …

Cite this