Stress-corrosion cracking of Al-Zn-Mg-Cu alloys effects of composition and heat-treatment

S. P. Lynch, S. P. Knight, N. Birbilis, B. C. Muddle

Research output: Chapter in Book/Report/Conference proceedingConference PaperOther

17 Citations (Scopus)
Original languageEnglish
Title of host publicationProceedings of the 2008 International Hydrogen Conference - Effects of Hydrogen on Materials
Pages243-250
Number of pages8
Publication statusPublished - 1 Dec 2009
Event2008 International Hydrogen Conference - Effects of Hydrogen on Materials - Jackson, WY, United States of America
Duration: 7 Sep 200810 Sep 2008

Publication series

NameProceedings of the 2008 International Hydrogen Conference - Effects of Hydrogen on Materials

Conference

Conference2008 International Hydrogen Conference - Effects of Hydrogen on Materials
Country/TerritoryUnited States of America
CityJackson, WY
Period7/09/0810/09/08

Cite this