Stress corrosion cracking of a wrought Mg-Mn alloy under plane strain and plane stress conditions

Bharat S Padekar, V S Raja, Raman Raghuvir Kumar Singh

Research output: Contribution to journalArticleResearchpeer-review

19 Citations (Scopus)
Original languageEnglish
Pages (from-to)180 - 193
Number of pages14
JournalEngineering Fracture Mechanics
Volume102
DOIs
Publication statusPublished - 2013