Stress corrosion cracking behavior of magnesium alloys EV31A and AZ91E

Bharat S Padekar, V S Raja, Raman Raghuvir Kumar Singh, Paul Lyon

Research output: Contribution to journalArticleResearchpeer-review

24 Citations (Scopus)
Original languageEnglish
Pages (from-to)169 - 176
Number of pages8
JournalMaterials Science and Engineering A: Structural Materials: Properties, Microstructure and Processing
Volume583