Pitting and stress corrosion cracking of stainless steels used in polymer processing

Wai Hoong Siew, Raman K Singh Raman, Barrington Charles Muddle, Nigel Cann, V Boicos

Research output: Chapter in Book/Report/Conference proceedingConference PaperResearchpeer-review

Original languageEnglish
Title of host publicationCorrosion & Prevention - 2004: Sustaining Industry
EditorsC Smith
Place of PublicationMelbourne Vic Australia
PublisherAustralasian Corrosion Association (ACA)
Pages112-1 - 112-10
Number of pages10
Publication statusPublished - 2004
EventAustralasian Corrosion Association (ACA) Conference 2004: Corrosion and Prevention - Perth, Australia
Duration: 21 Nov 200424 Nov 2004
Conference number: 44th

Conference

ConferenceAustralasian Corrosion Association (ACA) Conference 2004
Abbreviated titleCP 2004
Country/TerritoryAustralia
CityPerth
Period21/11/0424/11/04

Cite this