Microstructures of modified RR2072 single crystal superalloys and their effects on LCF response at 950 oC

Qizhi Chen, N Jones, David M Knowles

Research output: Contribution to journalArticleResearchpeer-review

Original languageEnglish
Pages (from-to)185 - 198
Number of pages14
JournalFatigue & Fracture of Engineering Materials & Structures
Volume26
Issue number1-2
Publication statusPublished - 2003