Microbiologically assisted stress corrosion cracking of carbon steel in mixed and pure cultures of sulfate reducing bacteria

Reza Javaherdashti, Raman Raghuvir Kumar Singh, Christopher Panter, Elena V Pereloma

Research output: Contribution to journalArticleResearchpeer-review

74 Citations (Scopus)
Original languageEnglish
Pages (from-to)27 - 35
Number of pages9
JournalInternational Biodeterioration and Biodegradation
Volume58
Issue number1
DOIs
Publication statusPublished - 2006

Cite this