Abstract
A Cu-10 vol% Cr in situ composite was produced by melt processing and deformed by swaging to form rods with a total deformation true strain of 3.15. Scanning electron microscopy showed that the composite microstructure consisted of Cr fibres aligned with their long axes parallel to the rod axis. X-ray diffraction indicated that the Cr fibres had a strong <110> fibre texture. The mechanical properties of the composite were measured by tensile testing over the temperature range -70 to 600°C. Examination of fibre fracture and fibre-matrix debonding at and near the tensile test fracture surfaces indicated that a transition from localised to global damage occurred between 300 and 400°C.
| Original language | English |
|---|---|
| Pages (from-to) | 3437-3447 |
| Number of pages | 11 |
| Journal | Journal of Materials Science |
| Volume | 38 |
| Issue number | 16 |
| DOIs | |
| Publication status | Published - 15 Aug 2003 |
| Externally published | Yes |
Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver