Caustic stress corrosion cracking of an SG cast iron in industrial Bayer liquor

Research output: Chapter in Book/Report/Conference proceedingConference PaperResearchpeer-review

Original languageEnglish
Title of host publicationProc. 14th International Corrosion Congress
Place of PublicationKelvin South Africa
PublisherCorrosion Institute of South Africa
Pages128.2/1 - 128.2/9
Number of pages9
ISBN (Print)0-620-239-433
Publication statusPublished - 1999
EventInternational Corrosion Congress 1999 - Capetown, South Africa
Duration: 26 Sep 19991 Oct 1999
Conference number: 14th

Conference

ConferenceInternational Corrosion Congress 1999
Abbreviated titleICC 1999
CountrySouth Africa
CityCapetown
Period26/09/991/10/99

Cite this

Singh Raman, R. K., Muddle, B. C., & Tomlins, R. M. (1999). Caustic stress corrosion cracking of an SG cast iron in industrial Bayer liquor. In Proc. 14th International Corrosion Congress (pp. 128.2/1 - 128.2/9). Corrosion Institute of South Africa.