@inproceedings{28ad8d4fec1943bcba7a5c2c404be07b,
title = "Caustic stress corrosion cracking of a mild steel and a cast iron: Does hydrogen play a role?",
author = "Singh, {Raman K} and Muddle, {Barry C}",
year = "2000",
language = "English",
isbn = "81-7764-086-0",
pages = "1051 -- 1061",
booktitle = "Materials Ageing and Life Management, Proc. Int. Symp",
publisher = "Allied Publishers Private Limited",
address = "India",
note = "Materials Ageing and Life Management ; Conference date: 01-01-2000",
}