Caustic stress corrosion cracking of a graphite cast iron component

Research output: Contribution to journalArticleResearchpeer-review

Original languageEnglish
Pages (from-to)199 - 206
Number of pages8
JournalEngineering Failure Analysis
Volume11
Publication statusPublished - 2004