Anodic polarization and stress corrosion cracking of mild steel in highly concentrated and hot caustic solutions

Raman K Singh Raman, Rihan Rihan, Matthew I Jeffrey, Barrington Charles Muddle

Research output: Chapter in Book/Report/Conference proceedingConference PaperResearchpeer-review

Original languageEnglish
Title of host publicationProceedings of the Corrosion Control and NDT Conference 2003
EditorsP Dove, et al
Place of PublicationMelbourne Vic Australia
PublisherAustralasian Corrosion Association (ACA)
Pages85-1 - 85-7
Number of pages7
ISBN (Print)0-9597454-4-0
Publication statusPublished - 2003
EventAustralasian Corrosion Association (ACA) Conference 2003: Corrosion Control and NDT Conference - Melbourne, Australia
Duration: 24 Nov 200326 Nov 2003
Conference number: 43rd

Conference

ConferenceAustralasian Corrosion Association (ACA) Conference 2003
Abbreviated titleCP 2003
CountryAustralia
CityMelbourne
Period24/11/0326/11/03

Cite this

Singh Raman, R. K., Rihan, R., Jeffrey, M. I., & Muddle, B. C. (2003). Anodic polarization and stress corrosion cracking of mild steel in highly concentrated and hot caustic solutions. In P. Dove, & et al (Eds.), Proceedings of the Corrosion Control and NDT Conference 2003 (pp. 85-1 - 85-7). Australasian Corrosion Association (ACA).