Original language | English |
---|---|
Title of host publication | Corrosion Science and Technology Mechanism, Mitigation and Monitoring |
Editors | U Kamachi Mudali, Baldev Jar |
Place of Publication | New Delhi, India |
Publisher | Narosa Publishing House |
Pages | 122 - 137 |
Number of pages | 16 |
Edition | First |
ISBN (Print) | 9788173199103 |
Publication status | Published - 2008 |
Advances in Generation of Design Data for stress corrosion Cracking
Research output: Chapter in Book/Report/Conference proceeding › Chapter (Book) › Research › peer-review